英语翻译制备接枝环氧树脂时,BPO最佳用量为占环氧用量的3%,环氧占共聚物最佳用量24%,丙烯酸占单体最佳用量19%;制备接枝环氧乳液时,各种试剂最佳配比为接枝环氧:乳化剂:溶剂:水=1:0.1:0.5:2
英语翻译
制备接枝环氧树脂时,BPO最佳用量为占环氧用量的3%,环氧占共聚物最佳用量24%,丙烯酸占单体最佳用量19%;制备接枝环氧乳液时,各种试剂最佳配比为接枝环氧:乳化剂:溶剂:水=1:0.1:0.5:2;制备复合乳液时,接枝环氧乳液与苯丙乳液复配最佳比例为2:8,涂膜表干时间16min,外观性能优良,涂膜硬度3H,耐水性260min,附着力1级
whenpreparinggraftepoxy,theoptimumamountofBPOaccountsfor3%oftheepoxy,epoxyaccountsfor24%ofcopolymer,acrylicaccountsfor19%ofmonomermixture;whenpreparinggraftepoxyemulsion,theoptimalratioofgraftepoxy,emulsifier,solventandwateris1:0.1:0.5:2;whenpreparingthecompositelatex,thebestratioofgraftepoxyemulsionandstyrene-acrylicemulsionis2:8,thedrytimeis16min,appearanceisexcellent,filmhardnessis3H,waterresistanceis260min,adhesionis1